1. … Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11 G-AlSi12 (Cu), …
  2. … Recommended for operating temperatures up to 1150° C in carburized low-Sulphur combustion gas, e. g. reforming ovens …
  3. … resistant up to 950ºC. Interpass temperature should be kept below 150ºC.  … 1.4828, 1.4829, 1.4893, 1.4835, 1.4818, 1.4825, 1.4826, …
  4. … low heat input and the interpass temperature should be limited to max. 150 °C. … 1.4898, GX45NiCrNbSiTi45-35  Parralloy H46M, Centralloy ET45, …
  5. … are kept above the minimum considered necessary to ensure satisfactory performance. SA 90S-B9 is best to be used with FL 880 high basic … A 387 Gr91 (plates), A 182 / A336 F91 (forgings), X10CrMoVNb 91, 1503 Gr91, AFNOR NF A-49213/A-49219 Gr TU Z 10, CDVNb 09-01 … SA 90S-B9 …
  6. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good corrosion-resistance and …
  7. … AA M400 offers a more dense and higher filling rate to obtain better performance and productivity. CEWELD® AA M400 can be used in a wide …
  8. … are kept above the minimum considered necessary to ensure satisfactory performance. In this case, weldments will be weakest in the softened …
  9. … The 0.5% alloying improves creep performance compared to CMn steels and sees the alloy being used for …
  10. … alloy with additions of Nb and V to improve high temperature creep performance. Interpass temperature: max. 300°C … alloy 24, 2.5%Cr1%Mo …