1. … without any risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing …
  2. … Solid drawn ,corrosion-resistant, chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, …
  3. … Dur CS consists of sintered tungsten carbide fragments in a ductile Nickel Bronze Silver matrix. The alloy has a tensile strength of …
  4. … tools, hardening is possible. The maximum hardness is dependent on the base metal and is often achieved in the first layer. … Rebuilding worn …
  5. … Excellent impact properties at low temperatures due to the addition of Nickel and increased yield strength above 460 MPa. … Materials …
  6. … the Nb carbides. The choice for the buffer layer is depending on the base metal and not always necessary. If applied correctly the …
  7. … Silicon bronze • Sound, pore free deposits on ferrous and non-ferrous base materials • Excellent corrosion resistance Best to be used with …
  8. … High Nickel-Chromium alloy with very good mechanical properties down to …
  9. … layer with AA M690 or AA M37-42 is recommended in case of sensible base material or old hardfacing layers. … HRc 58-62, Cement pumps, …
  10. … 450ºC. The recommended preheat temperature is 200ºC - 300°C unless the base material requires a higher preheat temperature. Use DC+ polarity …