1. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening …
  2. … CEWELD E 7024 (200) is a high performance electrode with a thick rutile coating and a recovery of …
  3. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening …
  4. … are kept above the minimum considered necessary to ensure satisfactory performance. In this case, weldments will be weakest in the softened …
  5. … are kept above the minimum considered necessary to ensure satifactory performance. … For matching P91, 9%Cr1%Mo modified, creep resisting …
  6. … both AC and DC+ with a recovery of 200% for excellent deposit performance. (Preheating is not required)Equivalent in FCAW: OA 59, OA …
  7. … be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or …
  8. … are kept above the minimum considered necessary to ensure satisfactory performance. In this case, weldments will be weakest in the softened …
  9. … AA M400 offers a more dense and higher filling rate to obtain better performance and productivity. CEWELD® AA M400 can be used in a wide …
  10. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable by special carbide tools, hardening …