Böhler CN 13/4-MC HI
Goede corrosiebestendigheid en slijtvastheid zoals vereist door waterturbines in waterkrachtcentrales.
1.4317, 1.4313, 1.4407, 1.4414,
GX4CrNi13-4, X3CrNiMo13-4, GX5CrNiMo13-4, GX4CrNiMo13-4
ACI Gr. CA 6 NM
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
0°C | |||||
As Welded | 800 | 890 | 19 | 67 | 40 HRc |