  2. … higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with OA 4370 or OA …
  3. … weld metal). Due to the addition of molybdenium suitable for post weld heat treatment respecting the impact properties. … Reh ≤ 620 MPa ISO …
  4. … slag in combination with very low hydrogen content. Suitable for heat treatment. Step cooling is possible. High reserve of toughness and …
  5. … Mechanical properties listed below reflect utilization of a post-weld heat treatment between 1020°C (1875°F) and 1050°C (1925°F) for one …
  6. … loss. Stable mechanical properties of the weld metal also at high heat input up to E …
  7. … grain boundary precipitation to maintain corrosion-resistance in the heat-affected zones of welded joints. Resistance to general, pitting …
  8. … hardness of 49-53 HRc at room temperature. The weld deposit is high heat resistant up to 900 °C. E Dur 12 offers a low coefficient of …
  9. … Extreme hard and heat resistant alloy that offers excellent cutting properties when …
  10. … Designed for welding heat resistant steels to sustain working temperatures up to 650˚C … For …