1. … with more deposit) No slag losses compare to 40% loss with standard electrodes.! Low amperage offers much lower heat input! 6 mm is ideal …
  2. … excellent all-position welding with higher currents. Applicable down to -40°C. Low spatter loss and remarkably easy slag removal. Due …
  3. … on metallurgical chemistry and excellent subzero impact properties down to -60°C. … Materials shipbuilding Unalloyed steels boiler steels …
  4. … weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  5. … purity, superior hot cracking and corrosion resistance. CVN toughness down to –120 °C, resistant to intergranular corrosion up to 400 °C. …
  6. … as wetting and reduce of spatter.  Excellent for use in position and down hand as well. The fast freezing slag unables CEWELD® AA 308LP to …
  7. … otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  8. … flux cored wire for extreme requirements at sub zero temperatures down to -60 °C. Excellent welding properties. Yield strength > 550 MPa. …
  9. … soundness and excellent slag removal.Excellent for use in position and down hand as well.High resistance against moisture pick up … Type 23 12 …
  10. … a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …