1. … alloy for use at operating temperatures up to (2100 °F) 1150 °C. It contains rare-earth additions for increased oxidation …
  2. … prior to welding. Heavy parts and thicker plates should be preheated (150 °C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., 99,5, …
  3. … covers a huge range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg4,5Mn, AlMg5, …
  4. … method during production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding Aluminium alloys …
  5. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, Al99,0 …
  6. … low heat input and the interpass temperature should be limited to max. 150 °C. … 1.4898, GX45NiCrNbSiTi45-35  Parralloy H46M, Centralloy ET45, …
  7. … anodizing. Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … AlMgSi 0, AlSiMg (A), AlSi 1 MgMn, …
  8. … Scale resistance up to 1150ºC, crack and wear resistant, suitable for rebuilding wornout parts. …
  9. … Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11 G-AlSi12 (Cu), …
  10. … Scale resistance up to 1150ºC, crack and wear resistant, suitable for rebuilding wornout parts. …