1. … subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The spray deposit is machinable by special carbide tools. … …
  2. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening …
  3. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening …
  4. … be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or …
  5. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable by special carbide tools, hardening …
  6. … Preheating and interpass temperature 400-450 °C (austenitic welding) or 250-300 °C (martensitic welding). Root passes should principally be …
  7. … subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The spray deposit is machinable by special carbide tools.  … …
  8. … impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening …
  9. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable by special carbide tools, hardening …
  10. … up to 450°C and offers scaling resistance up to 950°C. Preheating at 250 °C and stress relieving at 800 °C is recommended if this is …