1. … Due to the seamless manufacturing process, the content of diffusible hydrogen in the weld metal is extremely low (on average less than 3 …
  2. … metal due to the protective effect of the slag in combination with low hydrogen content Typical with FL 155 Flux … For matching P36 / W36 …
  3. … can be kept up to working temperatures of 600 ºC ; the hardness is still 40-45 HRc at these temperatures. For Hardfacing of more than 3 …
  4. … constructions that needs post weld heat treatment after welding and still offers excellent impact properties. … P235GH, P265GH, P295GH, …
  5. … metal conditioned by the high-basic slag in combination with very low hydrogen content. Suitable for heat treatment. Step cooling is …
  6. … FL 160 is a highly basic SAW flux with low hydrogen content. Basicity: about 3 (according to Boniszewski) Current: …
  7. … MPa yield strength steels, due to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long storage …
  8. … Extreme crack resistant weld deposit due to extra low hydrogen content when combined with Ceweld  FL 155. Developed for …
  9. … high general corrosion resistance. In media containing chloride and hydrogen sulphide, the alloy has a high resistance to intergranular …
  10. … the alloy a preferred choice in many applications to prevent or solve problems. The wire is cleaned in a very special way to provide a porous …