1. … The Welding Solution Center (WSC) is located at the Agro Park in Huissen and is part of … of new, innovative welding processes and procedures. The location (600 m2) accommodates the highest quality and innovative welding … offer your company, click here . Together with our partners we will present a number of issues during the year and we offer you the …
  2. … As earlier announced the new standard according EN ISO 1090 has entered the market  from the first of July … DNV, TUV, etc. of course our team is ready to support you with your pre-WPS and also with physical support and guidance during welding. … …
  3. … Alloy C276 is a popular nickel-molybdenum-chromium alloy renowned for its … corrosion-resistant weld.   Typical chemical composition in % Ni: 50-60 Cr: 14.5-16.5 Mo: 15-17 Fe: 4-7 W: 3-4.5 Co: ≤ 2.5 Mn: ≤ 1 Small … use in oil and gas processing environments where hydrogen sulfide is present. Alloy C276 is widely used in industries such as chemical …
  4. … Alloy 625 has high resistance to corrosion in both acidic and alkaline environments. It exhibits … encountered in chloride-containing environments. Alloy 625 finds widespread applications in industries such as chemical processing, …
  5. … Alloy 600 is a nickel-chromium alloy with good corrosion resistance to a wide range of … high temperatures and corrosion resistance. When welding Alloy 600, CEWELD® NiCro 600 can be used as filler material. This ensures … stress corrosion cracking, a type of corrosion that occurs in the presence of chlorides at elevated temperatures. Water Corrosion: Alloy …
  6. … These alloys are specially designed for high-temperature applications. They offer … chemical composition in % Ni: 30-35 Cr: 19-23 Fe: 39.5-42.5 Al: 0.15-0.60 Ti: 0.15-0.60 C: ≤ 0.10 Cu: ≤ 0.75 Small amounts of other elements … it suitable for applications in industries where sulfur compounds are present. Chloride-Ion Stress Corrosion Cracking (SCC) Resistance: Alloy …
  7. CEWELD® MA 600 (1.4718) offers outstanding abrasion resistance combined … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. … 600 HB, T Fe 8 … MA 600 (1.4718) … A 5.21: ERFeCr-A … 14700: T Fe8 …
  8. … This 99,0% pure aluminum filler metal offers excelent weldabillity and is the strongest in the 1000 series of the pure aluminium grades. Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the … 3.0275, 3.0257, EN AW 1200, EN AW 1050A, EN AW 1070A, EN AW 1350, 1060, 1070, 1080, and 3003. … Al99,0 … A 5.10: ER1100 … 18273: S Al 1100 …
  9. … Zirconium often is chosen for its resistance to corrosion from most … subsequent passes until the root surface temperature stays below 600 degrees F. Backup shielding also should be used on the back surface of sheet or plate less than 1/4 in. thick to prevent oxidation. Gas Requirements. Welding-grade argon (99.999 …
  10. CEWELD® E 6013 S is a medium thick coated electrode for all kinds of … suited for welding jobs at poorly accessible points and badly prepared seams. CEWELD® E 6013 S can be sued in all positions, in particular it is ideally suited …