- … grade of the Al-Bronze-types. Seawater-resistant copper-aluminum alloy without Zn with high toughness and improved hardness. “Very good …
- … losses of brazed joints with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low … … Copper to Copper (without flux). Brass, Copper and Copper-Tin Alloys (with flux). Do not use in a sulphurous environment. … L-Ag18PL …
- … Mechanical properties listed below reflect utilization of a post-weld heat treatment between …
- … 2400 HV nickel based corrosion resistant hardfacing alloy containing 60% tunsten carbides. OA WC2 (Ni) has excellent flow …
- … Very wel suited also for dissimilar welding between cast iron and high alloyed stainless and heat resistant steels or mild steels. Excellent …
- … combination of mechanical strength and corrosion resistance makes the alloy a preferred choice in many applications to prefent or solve …
- … high integrity structural service at elevated temperature so the minor alloy additions responsible for its creep strength are kept above the …
- … Outstanding alloy against abrasion, impact and high temperatures up-to 550 °C. The …
- … High Mn alloyed welding wire that can be used in combination with the fluxes FL …
- … flux for SAW welding to obtain increased hardness with low and un-alloyed sub arc wires. Basicity: about 1,1 (according to Boniszewski) …