- … sulfuric acid and many chloride containing media. This fluxcored wire may also find applications for joining Type 317L material where …
- … in a particular application or weldment. Other tests and procedures may produce different results. Users are cautioned to confirm by …
- … of high strength steels, used predominantly after stress relieving. May find its use for joining creep resistance steels up to about 500ºC …
- … of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where …
- … for such applications, where deleterious Nb-rich precipitates may form in diluted or partially mixed regions around the fusion …
- … significantly reduced when using AlSi12 as a filler alloy. The alloy may be used in applications at sustained elevated temperatures. …
- … of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where …
- … cracking. This alloy is often chosen to solve SCC problems, which may occur with 316L stainless … Alloy 20, Carpenter 20, 320 … 320 Tig … …
- … sulfuric acid and many chloride containing media. This fluxcored wire may also find applications for joining Type 317L material where …
- … metal in these zones, thus avoiding the risk of brittleness, which may sometimes occur when very thick welds are made (> 3 mm of sheet …