1. … Mpa) in case high impact values are required at sub zero temperatures. Hydrogen content HD < 4 ml/100 g. … Reh < 790 MPa  S620Q, S620QL, …
  2. … 525°C. Mostly used for the construction of boilers and pipes (15Mo3).Hydrogen content (HD < 5 ml/100 g). … Typ 0,5Mo   ISO 15608: ≤ 460 MPa …
  3. … such as with robots. Due to the seamless production process the hydrogen content is below 3ml/100g weld metal even after long storage. …
  4. … conditioned by the high-basicity slag in combination with very low hydrogen content. Well suited for the economic joining of fine grain …
  5. … the alloy a preferred choice in many applications to prevent or solve problems. The wire is cleaned in a very special way to provide a porous …
  6. … CrMoV-steels up to 550 °C. Due to the seamless production process the hydrogen content is below 3ml/100g weld metal even after long storage …
  7. … metal due to the high basic slag in combination with a remarkable low hydrogen content.  The requirements of the steels mentioned are …
  8. … on ceramic backing. Extreme low spatter loss, easy slag removal and hydrogen content below 3 ml/100gr. even after long unconditioned …
  9. … Remarkable crack resistant weld metal in combination with very low hydrogen content. Therefore, suitable for the economic processing of …
  10. … Remarkable crack resistant weld metal in combination with very low hydrogen content. Therefore, suitable for the economic processing of …