1. … fluidity (wetting action), making the alloy the preferred choice of welders. The alloy is not sensitive to weld cracking and produces bright, …
  2. … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall …
  3. … CEWELD® L-Ag49niMn is a very good flowing, low-melting silver hard solder for operating temperatures from -200 °C to Max. 200 °C (without … Super-Flux … Brazing tungsten tool tips, diamont, widia, and molybdenium alloys to steel … L-Ag49NiMn … A 5.8: BAg-22 … 17672: Ag 449 …
  4. … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In general the …
  5. … weld metal composition of 12% Chromium. These weld deposits are air-hardenable that can normally be heat-treated after welding. … 1.4000, …
  6. … better mechanical characteristics compare to standard PbSn soft solders.  Excellent results are obtained on stainless steel with our "ST" …
  7. … alter the surface electrochemistry of the material in the crevice or under a surface deposit. Grade 12 has better elevated temperature …
  8. … quality guarantees optimum metallurgical quality and attractive welder appeal. Combined with our high basic electro slag flux FL 830 ESHC …
  9. … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …
  10. … content (below 3 ml/100 gr. weld metal). Due to the addition of molybdenium suitable for post weld heat treatment respecting the impact …