1. … dissimilar welding between cast iron and high alloyed stainless and heat resistant steels or mild steels. Excellent Weldabillity with … and high resistance against porosity. The weld metal is corrosion and heat resistant. Very well suitable for welding with robotics or …
  2. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low heat input and the interpass temperature should be limited to max. 150 …
  3. … for welding grey, malleable, nodular and phosphorus cast iron. Preheat is not necessary. Heat input is low which favors limited heat affected zone. … GG, GGG Spheroidal Cast Iron, Diluted Cast Iron, …
  4. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low heat input and the interpass temperature should be limited to max. 150 …
  5. … Proper weldings are subject to the recommended heat treatment. The deposit is resistant to seawater, thin acids and … C. and will offer scale resistance up to much higher temperatures. Preheating is recommended at 150 - 350° C. depending on the thickness of the base metal. Similar base metals should be pre-heated at 300° C to 400° C. … 1.4016, 1.4511, 1.4122 X6Cr17,  X3CrNb17, …
  6. … better galling resistance. Normally to obtain adequate ductility, preheat and post-weld heat-treatment are required . AA 410 is a martensitic stainless steel that is heat-treatable. It has a nominal weld metal composition of 12% …
  7. … en er staat nog veel meer op stapel. … VERTROUW OP DE FILLER METAL SPECIALIST
  8. Brand: VAUTID
    CEWELD Product: OA 55 TC
    … 56 … VAUTID Delta