1. … metal provides optimum strength and oxidation resistance above 815 °C (1500°F) up to 1149 °C (2100°F), especially when welding on base metals …
  2. … method during production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding Aluminium alloys …
  3. … covers a huge range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg4,5Mn, AlMg5, …
  4. … is possible. High reserve of toughness and crack resistance. Flux FL 150 of FL 160 can be used in combination with this wire. … 2,25% Cr, 1% …
  5. … as alloy 59. The high level of Mo is similar to alloys C276 and C4 but performance in a wide range of more oxidizing media is significantly …
  6. … low heat input and the interpass temperature should be limited to max. 150 °C. … 1.4898, GX45NiCrNbSiTi45-35  Parralloy H46M, Centralloy ET45, …
  7. … CEWELD E 7024 (200) is a high performance electrode with a thick rutile coating and a recovery of …
  8. … aluminium grades. Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the benefits of …
  9. … are kept above the minimum considered necessary to ensure satifactory performance. … For matching P91, 9%Cr1%Mo modified, creep resisting … steels A 213 T91, A335 P91, A387 Gr91, A 182/A336 F91, X10CrMoVNb9-1, 1503 Gr91, AFNOR NF A-49213/A-49219 Gr TU Z 10, CDVNb 09-01 … ER 90S-B9 …
  10. … are kept above the minimum considered necessary to ensure satisfactory performance. In this case, weldments will be weakest in the softened …