1. … buffer layer except on materials considered critical or in case of old hardsurfacing layers. The weld deposit can be aplied completely crack …
  2. … abrasion combined with impact. The deposit gives already a very good hardness in the first layer. The choice for the buffer layer is depending on the base metal and not always necessary.  … 55-57 HRc hardfacing alloy against shocks and mineral wear, rollers and crushers, …
  3. … for the repair of the capillary losses of brazed joints with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding …
  4. … copper-aluminum alloy without Zn with high toughness and improved hardness.  “Very good weldability compare to the more common Al. …
  5. … even at higher temperatures. The deposit gives already a High hardness in the first layer. A buffer layer is recommended in case of … protective gas.Corresponding electrode: CEWELD® Dur 62 S … 61-64 HRc hardfacing alloy, Cement, Mineral mixing, hammers, coke wear plates …
  6. … sea water, salts and reducing acids. The weld metal is not age hardenable and when used to join Monel K-500 it has lower strength then …
  7. … and corrosion at high working temperatures upto 900°C. Crack free hard facing deposit against severe shock and impact. … CoCr-E  Co1 …
  8. … and Powder HVOF DUR 1 (45/15). It contains a higher fraction of hard, brittle carbides than Powder HVOF DUR 6 (45/15), and has … pump vanes, bearing bushes and narrowneck glass mold plungers. Hardfacing of engine valves, pinch rollers in the metal-processing …
  9. … Very good corrosion resistance combined with high hardness even at higher temperatures. Excellent weldability and often …
  10. … of tungsten carbides embedded in a steel matrix. The extraordinary hardness of the fused tungsten carbides (WSC) of approx. 2300 HV imply …