1. … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall …
  2. … rutile slag with which X-ray weld seams are reliably achieved both under CO2 and mixed gas … ISO 15608: 8.1  Austenit ≤ 19 % Cr , TÜV 1000: …
  3. … optimum deposit rate and metallurgical quality and attractive welder appeal in the PA-PB position. Very good resistance against pitting …
  4. … fluidity (wetting action), making the alloy the preferred choice of welders. The alloy is not sensitive to weld cracking and produces bright, …
  5. … CEWELD dans plus de 60 pays à travers le monde.  Au cours de la dernière décennie, un grand nombre de nouveaux alliages ont été …
  6. … quality guarantees optimum metallurgical quality and attractive welder appeal. Combined with our high basic electro slag flux FL 830 ESHC …
  7. … DC. The carbon content of the base metal should not exceed 0,45 % in order to avoid lack of fusion.  … Scratchers, Mixers, Deep drilling, …
  8. … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …
  9. … all weld metal requires no buffer layer except on materials considered critical. Suited for wear parts subject to heavy impact and … first layer.  … Conveyors and transport surfaces, tires, bucket and loader teeth, cruscher jaws, Bufferlayers, crane wheels, axis, gear parts, …
  10. … all spray metal requires no buffer layer except on materials considered critical. In this  Situation …