1. … from porosity due to the special shaving process and cleaning method during production. AlMg5 is one of the most popular types within the …
  2. … sont de plus en plus appréciés par les clients dans le monde entier. Pour renforcer notre présence, nous avons ouvert des succursales en …
  3. … It is self bonding to most materials and requires minimal surface preparation. Bond strengths in excess of 9000 psi can be achieved on …
  4. … from porosity due to the special shaving process and cleaning method during production. AlMg4,5Mn is one of the highest grades within the …
  5. … "NiLo'" and offer the lowest schrinkage possible to avoid cracks during heating and the cooling period. The weld deposit also retains …
  6. … less than 1% nickel to full fill NACE requirements and cover more procedures up to 500 MPa yield strength steels. CEWELD® AA M500 can also be … 65, Oceanfit 355, Oceanfit 420, Oceanfit 460, alform plate 460M; durostat 400, 450, 500, durostat B2     … AA M500 … A 5.28: E80C-Ni1 H4 … A 5.36: …
  7. … 50 kVA et notre machine à induction ProHeat 35 avec Rolling Inductor, pour le préchauffage du manipulateur. Outre l'exécution de ces …
  8. … root of the weld on the first pass and blankets the solidified weld during subsequent passes until the root surface temperature stays below …
  9. … Weldable without protective gas.Corresponding electrode: CEWELD® Dur 62 S … 61-64 HRc hardfacing alloy, Cement, Mineral mixing, hammers, …
  10. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Grey Cast Iron, …