1. … The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall a temperature of 1000°C be …
  2. … The alloy has a low carbon content, making it particularly recommended where there is a risk of intergranular corrosion. The fast …
  3. … This results in lower hardness and strength values, which reduces the tendency to crack, especially if the weld seams are not …
  4. … to 950°C. Preheating at 250 °C and stress relieving at 800 °C is recommended if this is permissible for the base metal. In the machined state …
  5. … A Buffer layer with CEWELD® OA 4370 or CEWELD® OA MnCr is recommended in case of old layers or critical base metals. Weldable with M21 …
  6. … already a High hardness in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without …
  7. … hardness in the first layer. The choice for the buffer layer is depending on the base metal and not always necessary.  … 55-57 HRc …
  8. … The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. can  be used …
  9. … The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The higher …
  10. … Equivalent) is over 40. Ar-CO2 mixed gas or 100%CO2 is recommended as shielding gas for excellent weldability. … 1.4507, 1.4410, …