1. … offering satisfying results although the old method (pressing twice) still offers the best weldability, but a special press is needed and …
  2. … stress corrosion cracking. This alloy is often chosen to solve SCC problems, which may occur with 316L stainless … Alloy 20, Carpenter 20, …
  3. … temperature and post weld treatment as required for the base metal. Hydrogen content: HD < 3 ml / 100 g weld metal. CEWELD E 11018-H is …
  4. … metal conditioned by the high-basic slag in combination with very low hydrogen content. Suitable for heat treatment. Step cooling is …
  5. … extreme deposition rates. Due to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long …
  6. … up to 550 °C (1022°F) . Due to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long storage …
  7. … Excellent against pitting and stress corrosion. The PREN above 35 weldmetal offers outstanding resistance against pitting. … ISO 15608: …
  8. … FL 830 ESH has an excellent slag removal. Flux has a low hydrogen potential which makes it suitable for overlay welding of heat …
  9. … corrosion and oxidation and suitable for applications when exposed to hydrogen sulfide or sulfur dioxide. … The nominal composition (wt.-%) …
  10. … acid at all concentrations and tempertures. It also withstands hydrogen chloride, sulfuric, acetic, hydrofluoric nd phosphoric acids. …