- … was originally targeted for use as A-USC boiler tubes in the superheater sections of these plants but was then adapted for application as …
- … it is able to meet the set requirements very economically with high heat input. For more information, please refer to our brochure or …
- … Excellent weldability, and can be heat treated to a higher strength or toughness. Grade 5 is used in …
- … with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low operating temperature. …
- … wires. Excellent weld metal quality and X-ray soundness. Post weld heat treatment (PWHT) can be applied without any problems. … 19% Cr / …
- … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. AA …
- … hardness of 49-53 HRc at room temperature. The weld deposit is high heat resistant up to 900°C. DUR 12 offers a low coefficient of friction …
- … to be used in corrosive environments, normally without post-weld heat treatment. At 33% nickel, CEWELD® 320 Tig has practical immunity …
- … and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg3, AlMg4, …
- … a full high hardness in the total thickness of the plate. No excessive heat that effects the basemetal or cause loose in strength two times …