1. … to NILO Alloy 36, while providing freedom from solidification and reheat cracking. NILO Alloy 36 is available for Tig, Mig and SAW process. …
  2. … CEWELD 4332-Ti is a rutile basic electrode for joining heat resistant CrNi-steels of the same kind and also joining dissimilar …
  3. … is resistant against impact wear as well as permanent stress by heat influence, metal wear and high surface pressure  … 1.4317, 1.4313, …
  4. … grain boundary precipitation to maintain corrosion-resistance in the heat-affected zones of welded joints. Resistance to general, pitting …
  5. … and corrosion resistance even in seawater. Welding instructions: - Preheating for sections >6 mm from 150 till 300 ºC is recommended. Use the …
  6. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150 °C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., …
  7. … and cleaning method during production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding Aluminium …
  8. … deposit is capable of taking a high polish. Structure: Austenite with delta ferrite … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) / E347, 19 9 …
  9. … CEWELD AA M460 can also be used for constructions that needs post weld heat treatment after welding and still offers mechanical properties …
  10. … Suitable for cladding and joining components against corrosion, high-heat and wear resistance. Weldable with the Sub-Arc process using … Cr-Al-Si steels., cladding corrosion resistant overlays., Cladding heat resistant overlays (1100ºC), Cladding components in a sulphurous …