1. … to crack, especially if the weld seams are not heat-treated.These steels are usually used for operating temperatures of up to 550°C. … … For similar 1.25%Cr-0.5%Mo-alloyed, heat-resistant, ferritic steels. 1.7335, 1.7242, 1.7337, 1.7357 13CrMo 4-5, 13CrMo 4-4, 16 …
  2. … 350 Kb that delivers a welding deposit of less hardness. Overlays on steel with high tensile strength should be buffered with CroNi 29/9 HL …
  3. … chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. CEWELD 310 has good general …
  4. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down …
  5. … A Rutile basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. 2209 has high … in a variety of applications across all industrial segments.  … Duplex stainless steels,  1.4462, 1.4417, 1.4582, 1.4463, 1.4460, 1.4362, 1.4583, 1.4162 …
  6. … spatter loss, easy slag removal. Well suited for joining high carbon steels and when welding critical mixed base metal combinations. Ideal … C, D, A 830 M, A 516 M, A 299 M, A 573 M UNS G10220, SAE 1022 Armco Steels, Telar 75 … AA B350 … A 5.20: E61T-G … 17632-A: T 35 4 B M 1 H5 …
  7. … Basic electrode for weather resistant steel such as, Patinax, Corten, Acor 50, HSB 51, etc. Excellent …
  8. … alloy is often chosen to solve SCC problems, which may occur with 316L stainless … Alloy 20, Carpenter 20, 320 … 320 Tig … A 5.9: ER320 … …
  9. … of high-strength and low temperature fine grained structural steels. Excellent welding properties in combination with FL 155 high … 700, Dilimax, Naxtra 70, 10CrMo9-10, 16NiCrMo12-6, high strenght steels with yield >690N/mm2, S500Q-S690Q, S500QL-S690QL, P500Q-P690Q, …
  10. … Hardfacing alloy for cladding steel mill rollers, thermoshock resistant and suitable for Francis and …