1. … oxidation and abrasion, and excellent resistance to impact and bending. SP 80/20 NiAl can be machined and ground to a finish of 5 micro …
  2. … not be deposited. A Buffer layer with OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. Equivalent in …
  3. … The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall a temperature of 1000°C be …
  4. … coatings on steel substrates. Furthermore, the aluminum coating tends to form an oxide film that protects it from further attack. … … on components such as conductive areas on insulators, capacitor end caps and varistors. Cathodic corrosion protection on steel, …
  5. … to avoid cracking. A buffer layer with OA 4370 or OA MnCr is recommended in case of sensible basematerial or old layers. Weldable without …
  6. … where high temperature properties are required. It is not recommended to use this alloy for welding aluminium alloys with a high …
  7. … layer. A buffer layer with CEWELD® OA 4370 or CEWELD® OA MnCr is recommended in case of sensible basematerial or old hardface-layers. Weldable …
  8. … or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing layers should be removed, clean or …
  9. … minimize the heat input, because materials of this composition have a tendency to embrittle in the temperature range of approx. 600-800° C. …
  10. … low alloyed steels with tensile strength up to 510 N/mm2. Recommended for root welding in pipelines due to excellent welding …