1. … 2400 HV nickel based corrosion resistant hardfacing alloy containing 60% tunsten …
  2. … without any risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing …
  3. … layer with OA 4370 or OA MnCr is recommended in case of sensible basematerial or old layers. Weldable without protective gas.  … HRc …
  4. … AA R500 SR is a seamless rutile cored wire and has excellent modelling ability, therefore …
  5. … The particles should fall before the solidification in the molten weldpool and … sawing steel and concrete, deepsea wrack sawing, mixing paddles, scraper blades, mining etc.... … DUR WC 3000 …
  6. … heat-resistant steels and steel-castings. The weld-deposit is on equal base-material scale-resistant and, by reason of its low nickel-content, …
  7. … and when used to join Monel K-500 it has lower strength then the base metal. … 2.4360, 2.4375, NiCu30Fe, NiCu30Al, Monel 400, R405, …
  8. … The deposit is free from porosity even on old and or otherwise diluted base material. Preheating is normally done to slow down the cooling …
  9. … SACW460-1W is a cored wire with micro-alloy elements, which enables welding of one side with one layer and layer counter layer with …
  10. … Titanium carbides. The choice for the buffer layer is depending on the base metal and not always necessary.  … HRc 54-59, hardfacing alloy for …