1. … repair sector due to its absolute insensitiveness for rust or diluted base metals. Hydrogen content: HD < 10ml/100g weld metal. … Reh ≤ 420 … A 841 Gr. A; API 5 L Gr. B, X42, X52, X56, X60, Domex 315-420MC,MC Plus, ML  … E 7016 … A 5.1: E 7016 … 2560-A: E 42 4 B 12 H10 …
  2. … Stainless steel with excelent resistance to intercrystalline corrosion and …
  3. … It has cavitation-erosion resistance ten times that of 304 stainless steel, Dur 12 can be used to protect bearing surfaces in …
  4. … Special alloy for welding aluminium-magnesium based alloys with maximum 5% Mg. Zirconium added as grain refiner to …
  5. … It has cavitation-erosion resistance ten times that of 304 stainless steel, E Dur 12 can be used to protect bearing surfaces in …
  6. … Sound, pore free deposits on ferrous and non-ferrous base materials offering excellent resistance to corrosion in sea water. …
  7. … OA 4370 or OA MnCr is recommended in case of old layers or critical base metals. Equivalent in SMAW: Dur 64 … For fire gratings, sintering …
  8. … CEWELD® 410 Tig is a martensitic stainless steel that is heat-treatable. It has a nominal weld metal …
  9. … interpass temperature and post weld treatment as required for the base metal. Hydrogen content: < 3 ml / 100 g weld metal. …  < 620 MPa …
  10. … 16,000 hours. Suitable for joining and cladding Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X …