1. … Eutectic alloy self pickling on copper. Exceptional fluidity. It is very … losses of brazed joints with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low … … Copper to Copper (without flux). Brass, Copper and Copper-Tin Alloys (with flux). Do not use in a Sulphurous environment. … L-Ag18P … …
  2. … CEWELD 4820 AC is an AC-weldable fully core-wire alloyed electrode for fabrication and repair welding on equal or … to 1150 °C. When welding CEWELD 4820 AC low heat-input is required as alloys of such chemistry are sensitive to embrittlement at 600-800 °C. …
  3. … and N additions provide this ‘creep strength enhanced ferritic’ (CSEF) alloy with improved high temperature creep resistance compared to standard CrMo creep resistant alloys. … For matching P92, 9%Cr1.7%W0.5%Mo, creep resisting …
  4. … Melting Point 1112°F, Magnesium 92/8 is Mg - 9 Al - 2 Zn welding alloy which finds wide use for fabricating and repair welding of many … application.Magnesium 92/8 is preferred for joining many casting alloys. … Magnesium alloys, 2L124, 2L125, L122. AMS 4484, 4434, 4453, AZ31B, AZ10A, ZK21A, …
  5. … product consisting of crushed tungsten carbide and a Ni-based alloy. Crushed cast carbide will guaranty a long life. Furthermore the Ni-based alloy provides an excellent corrosion resistance. E DUR RU (Ni) has …
  6. … an agglomerated flux for SAW welding stainless steels and Nickel based alloys: AISI 2205, Alloy 625, 904L Basicity: About 1,7 (according to Boniszewski) Current: …
  7. … seawater and against fouling. Suitable for dissimilar welding of Monel Alloy 450 to Nickel 200 and or other Copper -Nickel alloys. Small diameters can be used in all positions. … Cu7158 … 2.0838 Mat.n: 2.0878, 2.0882,  (Monel 67): Wrought and Cast Alloys of 70-30, 80-20 and 90-10 Copper Nickel Alloys, Monel Alloy 450, …
  8. … especially at high temperatures, due to its high Cr content. The alloy is fully austenitic and is therefore sensitive to hot cracking. … for use under intermittent oxidation depend on cycle frequency. This alloy can withstand relatively severe thermic shock, and is superior to …
  9. … Mn, Ni, Cr and Mo alloyed basic electrode for welding low alloyed steels with tensile strength > 620 MPa. Crack resistant and …
  10. … A stainless steel alloy for the assembly and cladding of 17% chromium alloys and age Hardfacing components where heat and corrosion …