1. … in the molten weldpool and become part of the weld deposit, Metal core fluxcored wires are recommended in spray arc to obtain the …
  2. … The filler metal has low levels of tramp elements (eg. Sn, As, Sb and P) providing …
  3. … tensile strenght and a high resistence against sliding wear of metallic objects.It has a good retention of hardness up to 650°C and is …
  4. … Due to the high resistance to cracking and toughness, all spray metal requires no buffer layer except on materials considered critical. …
  5. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat resistant up …
  6. … with corresponding flux.  Suitable fluxes are depending on the weld metal requirements, in most cases CEWELD® FL 155 gives excellent …
  7. … better wetting properties compared to solid wires. Excellent weld metal quality and X-ray soundness and excellent slag removal. … 19%Cr, …
  8. … first layer. The choice for the buffer layer is depending on the base metal and not always necessary.  … 55-57 HRc hardfacing alloy against …
  9. … arc. Good slag removability and fine flaky seam pattern. The weld metal is high-temperature resistant with very good creep resistance. …
  10. … Filler metal with good flowing properties and capillarity.  Colour very …