1. … sub zero temperatures down to -60°C. CTOD tested and suitable up to steel types with 460 MPa yield strength (such as S460), approved …
  2. … is a bronzed wire to offer excellent feeding properties with standard steel liners. … S185-E360, S235JR-S355JR, S235J0-S450J0, S235J2-S355J2, …
  3. … spatter loss, easy slag removal. Suitable for economic welding of Mo-steels up to 500°C. … Typ 0,5Mo  ≤ 460 MPa,  ISO 15608: 1.2, 1.3 …
  4. … for welding fine grained similar alloyed high yield strength steel ( < 830 Mpa) in case high impact values are required at sub …
  5. … range of nickel alloys. Nickel based welding wires that are covered in AWS A 5.14 such as alloy 82, Inconel 600, 625, 601, 825, C276, alloy 59 … Grain size: 2-16 … Nickel based welding wires that are covered in AWS A 5.14 such as alloy 82, Inconel 600, 625, 601, 825, C276, alloy 59 …
  6. … chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. 310 has good general oxidation …
  7. … corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. CEWELD 2209 Duplex …
  8. … in case of rebuilding but heat input should be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or rebuilding parts that are subject to high impact and rolling …
  9. … TIG/GTAW rod for T24 creep resistant steel. The T24 alloy is a modified 2.25%Cr1%Mo alloy with additions of … max. 300°C … alloy 24, 2.5%Cr1%Mo modified, creep resisting ferritic steels. X7CrMoVTiB 10-10 1.7378 / 7CrWVMoNb9-6 - 1.8201 ASTM: A/SA 335 …
  10. … Mn, Ni, Cr and Mo alloyed basic electrode for welding low alloyed steels with yield strength > 690 MPa. Crack resistant and well suited …