1. … can be kept up to working temperatures of 600 ºC ; the hardness is still 40-45 HRc at these temperatures. For Hardfacing of more than 3 …
  2. … Welding instructions: - Preheating for sections >6 mm from 150 till 300 ºC is recommended. Use the normal standard welding techniques. …
  3. … constructions that needs post weld heat treatment after welding and still offers excellent impact properties. Due to the seamless production …
  4. … against heavy abrasion. Usualy the maximum number of layers is 2 till 3 but when using a special stringer build up technick with release …
  5. … will remain very well at increased temperatures. Scale resistant till 900°C.CEWELD MA 617 is best to be used with Ar/Co2 - 98-2.  … …
  6. … Zuverlässigkeit und Innovation auf höchstem Niveau ausgewählt. Ab 2017 sind die folgenden Schweißverfahren & Produkte in der Praxis …
  7. … constructions that needs post weld heat treatment after welding and still offers mechanical properties confirming 5Y46 class. Due to the …
  8. … constructions that needs post weld heat treatment after welding and still offers excellent impact properties. … P235GH, P265GH, P295GH, …
  9. …                           3 Layer: 61 - 65 HRc For the best results 2 till 3 layers should be welded. … Sugar mill knives and Hammers, Cement …
  10. … The weld deposit is offers strain hardening properties from 250 till 450 HB … austenitic manganese steel, high impact loads, hammers, …